Blocking in blown film (film adhesion) is a common problem encountered by many manufacturers, which not only affects products’ quality, but also reduces production efficiency. So what is the main cause of this phenomenon and how to deal with it? Let’s find out in this article. 

Blown film is one of the most popular plastic manufacturing methods worldwide. As it offers end-products great uniform properties regarding the length and width, it is specifically preferred in the packaging industry. However, its effectiveness also comes at the cost of unexpected problems, which include film blocking. 

1. Blocking in blown film: What is it?

Blocking in blown film is the adhesion of two adjacent layers of film. It is most frequently seen in polyethylene and polypropylene film processing (either blown or cast), and to a lesser extent in extrusion-coated or laminated products. 

Blocking in blown film: Main causes and solutions
Blocking in blown film is the adhesion of two adjacent layers of film

2. How to measure blocking in blown film?

Measuring the tendency blocking in blown film allows manufacturers to provide timely solutions to minimize the negative impacts on end-products. There are various test methods for measuring the tendency of a film to block.

In production, a very simple manual test is often carried out in which two layers of a film are placed on top of each other and moved between thumb and index finger or separated from each other.

Also, blocking in blown film can be estimated using a standardized scientific method (ASTM D-3354-89). The force required to separate two films is measured. The individual layers of the foil are each applied to an aluminium block, one of the blocks being attached to the base of the apparatus and the other block (weight-compensated) being mounted on a balance arm. On the opposite side of the scale arm, weights can be applied to increase the force until the layers of film separate.

3. What causes blocking in blown film?

Blocking in blown film can be resulted from various parameters. Here are top factors that can lead to this problem.

Thermodynamic parameters (temperature, cooling capacity)

Blocking in blown film: Main causes and solutions
Thermodynamic factors are main causes of blocking in blown film
  • Thermodynamic process control of cooling is decisive (coolant temperatures, volume flows)
  • Reaching a special critical temperature level before winding (depending on the material)
  • For thicker films, it is not the surface temperature that is decisive, but the core temperature (since the heat on the roll migrates from the inside to the outside and can then lead to blocking)
  • Inline drying times are not observed, are uncontrolled or incorrectly parameterised
  • Automated adaptation of cooling process parameters for different processes, products, hall temperatures or other environmental influences can often increase the productivity of a plant and keep its quality robustly high
  • Computer simulations provide insight into the process

Mechanical parameters (contact force, tension)

  • Winding tension is too high

Tension levels can easily be overlooked unless they are so great the core is crushed, making it impossible for the operator to remove the roll from the winder shaft. If the core is crushed only slightly, the operator may be able to remove the core from the shaft, but you may then find it impossible to remount it on a let-off stand. Just as bad a problem can arise if the winding tension is too low, blocking will not occur, but the film may telescope out from one end of the roll, making the film impossible to convert.

  • Winding tension is not adjusted with increasing winding diameter, but is constant
  • Contact force of pressure rollers is too high

Technical material parameters

  • Non-optimal proportion of antiblocking agents 
  • Inappropriate type of antiblocking agent 

If the additive levels are designed for a 4-mil film and you are producing a 1- mil film, not enough slip and antiblock additives are present to prevent blocking in blown film from occurring.

Blocking in blown film: Main causes and solutions
Wrong type of antiblocks results in insufficient use
  • Lubricant migration takes place
  • Incorrect binder (printing)
  • High residual solvent content (printing) 
  • Unsuitable compound 

Machine

  • Setpoints are not exactly maintained
  • Control behaviour leads to overshooting or undershooting
  • Defective, incorrectly parameterized or scaled sensor values
  • Lack of positioning accuracy

Management

  • Lack of knowledge about the influence of the machine operator
  • lack of time for process optimization
  • lack of time for quality monitoring
  • Lack of internal training 

4. Anti-blocking additive - effective solution to blocking in blown film

Anti-blocking additives are substances added in blown film manufacturing process to prevent the adhesion between film layers. By creating micro-rough surfaces, they can lessen the bond between film layers and minimize the tendency of the blocking in blown film. The effectiveness of anti-blocks is determined by two factors: the number of particles of antiblock at the film surface and the size of the antiblock particles. Proper selection of additive type somehow depends on the thickness of the film. 

Blocking in blown film: Main causes and solutions
Anti blocking additives

Generally, anti-blocking additives are divided into two main types, which have different characteristics.

Inorganic anti-blocking additives

These are non-migratory additives which are useful for high temperature applications since they melt at much higher temperatures than typical polyolefin extrusion temperatures. The biggest advantage of this type is its reasonable price, making it an ideal choice for large volume, commodity-like applications.

The table below summarizes a variety of inorganic materials typically considered for antiblock use:

Type Description
Natural silica (DE) Silicon dioxide (SiO2) - Mined
Talc Magnesium silicate - Mined
Synthetic silica Silicon dioxide - Manufactured
Calcium carbonate Calcium carbonate (CaCO3) - Mined
Ceramic spheres Alumina-silicate ceramic - Manufactured
Kaolin/clay Aluminum silicate - Mined
Mica Aluminum potassium silicate - Mined
Inorganice materials for antiblock use

Organic anti-blocking additives

Organic antiblocks are migratory in nature. They function by crystallizing on the film surface, thus forming interfering layers between the adjacent film layers. Organic antiblocks are of interest in high clarity films and “release” applications (e.g. for rubber bales or sticky food items). Compared to its counterpart, organic anti-blocking additives are more expensive. Therefore, they are much preferred in higher value-added applications. 

5. EuroPlas anti-blocking additives

After 14 years of development, EuP has demonstrated its strong position in the plastic material market. We take pride in providing customers with the highest quality additives including anti-blocks. Thanks to outstanding advantages, EuroPlas anti-blocking additives are widely used in various applications. Most importantly, our additives are tailor made based on your requirements, making them the right fit for your products. 

For further information and consultation, contact us!

 
News Other
PBS Plastic: Definitions and Applications You Should Know
Comprehensive guide to PBS plastic covering its definition, properties, and applications. Understand its role in advancing sustainable materials and processes.
TPU Plastic: What You Need To Know
Discover all about TPU plastic and the surprising benefits of TPU plastic in life.
Polystyrene Sheets in the Arts and Crafts Industry
Discover the versatility of polystyrene sheets for crafting, construction, and insulation. Lightweight, durable, and customizable for endless applications!
The Role of PS Material in Modern Industry
Facing material efficiency and cost challenges? PS material offers versatile solutions to boost performance and sustainability. Explore today! 
 
PBAT vs. PLA: How To Know The Right Plastic?
Learn the key differences between PBAT vs PLA to choose the perfect eco-friendly plastic for your needs and cost-effectiveness!
arrow_upward